عنوان انگلیسی Effects of three different mouthwashes on the surface characteristics of nickel-titanium and Stainless steel archwires in orthodontics
چکیده انگلیسی مقاله Introduction: Patients are recommended regular using of mouthwashes to control dental caries or periodontal diseases since orthodontic treatment may have detrimental effects on the tooth structures. However, chemical agents may potentially damage metal components of orthodontic appliances. The aim of this study was to evaluate the influence of three mouthwashes on the surface characteristics of nickel–titanium (NiTi) and Stainless steel (SS) arch wires. Methods and Materials: 15 pieces of 0.016 inch NiTi and 15 pieces of 0.016-inch SS wires were randomly assigned into 5 groups including 2 controls (as- received and artificial saliva) and 3 experimental groups. The samples in all groups were stored in artificial saliva in an incubator at 37˚C for one month, after that, the test groups were immersed in Chlorhexidine 0.12%, Hydrogen peroxide 0.12% and Persica mouth washes for 30 min, 1.5 h and 1.5 h, respectively. Then, the samples were washed by distilled water and returned to artificial saliva for more than two months. Surface topography changes and the number of corrosion holes were characterized via a scanning electron microscope (SEM).Two way ANOVA and Tukey tests were used to compare groups. Results: SEM photographs of the present study showed significant corrosion rate among "as- received" group and Persica (p=0.04), Chlorhexidine (p=0.02), and artificial saliva group (p=0.008) in NiTi wires, but there was no significant difference in the surface topography between any of the groups in SS wires. Conclusion: Alterations in surface of NiTi wires were significantly more than SS wires. Although not significant, 0.12% Chlorhexidine and Peroxide showed higher pitting view on SS and NiTi wires, respectively compared to other mouthwashes
کلیدواژه‌های انگلیسی مقاله Mouthwashes, Nickel-titanium, Orthodontics, Stainless steel

نویسندگان مقاله مریم امیدخدا | maryam omidkhoda
dental materials research center, associate professor, department of orthodontics, faculty of dentistry, mashhad, iran


مریم پوستی | maryam poosti
assistant professor, orthodontic department, school of dentistry, islamic azad university of medical sciences, tehran, iran

سازمان اصلی تایید شده: دانشگاه آزاد اسلامی علوم و تحقیقات (Islamic azad university science and research branch)

ضحی صاحب نسق | zoha sahebnasagh
assistant professor, department of oral and maxillofacial radiology, school of dentistry, zahedan university of medical sciences, zahedan, iran

سازمان اصلی تایید شده: دانشگاه علوم پزشکی زاهدان (Zahedan university of medical sciences)

سید مجتبی زبرجد | seyed mojtaba zebarjad
department of materials science and engineering, engineering faculty, shiraz university, shiraz, iran

سازمان اصلی تایید شده: دانشگاه شیراز (Shiraz university)

زهرا صاحب نسق | zahra sahebnasagh
assistant professor, department of oral and maxillofacial radiology, school of dentistry, zahedan university of medical sciences, zahedan, iran

سازمان اصلی تایید شده: دانشگاه علوم پزشکی زاهدان (Zahedan university of medical sciences)


نشانی اینترنتی http://jdmt.mums.ac.ir/article_8106.html
فایل مقاله اشکال در دسترسی به فایل - ./files/site1/rds_journals/278/article-278-314909.pdf
کد مقاله (doi)
زبان مقاله منتشر شده en
موضوعات مقاله منتشر شده
نوع مقاله منتشر شده 1
برگشت به: صفحه اول پایگاه   |   نسخه مرتبط   |   نشریه مرتبط   |   فهرست نشریات