عنوان انگلیسی Optimized Leaching Conditions for Selenium from Sar-Cheshmeh Copper Anode Slimes
چکیده انگلیسی مقاله The recovery process of selenium from Iranian Sar-Cheshmeh copper anode slimes employing hydrometallurgical methods has been investigated. The copper anode slimes are made up of those components of the anodes, which are not soluble in the electrolyte. They contain varying quantities of precious metals like gold, silver, selenium and tellurium. They are being extracted as a by product in the copper production process.In this paper, some parameters affecting the leaching conditions of anode slimes in nitric acid are studied. Taguchi experimental design method is used to find out the effect of acid concentration, temperature and time.The statistical results of the experiments show that the above parameters are important in the leaching of -10 microns fraction. The optimum conditions determined are: T = 90º C, acidity = 4 M and the leaching time = 60 min. Under these conditions, 99 % of the selenium is leached out.
کلیدواژه‌های انگلیسی مقاله

نویسندگان مقاله محمود عبدالهی |
mineral processing group, tarbiat modarres university, p.o. box 14115-143, tehran, i.r. iran
سازمان اصلی تایید شده: دانشگاه تربیت مدرس (Tarbiat modares university)

سید ضیایالدین شفایی | seid ziadin
mining department, technical university of shahrood, shahrood, i.r. iran


نشانی اینترنتی http://www.ijcce.ac.ir/article_8144_4f0448024155e268e4a94d7c05858ee5.pdf
فایل مقاله فایلی برای مقاله ذخیره نشده است
کد مقاله (doi)
زبان مقاله منتشر شده en
موضوعات مقاله منتشر شده
نوع مقاله منتشر شده
برگشت به: صفحه اول پایگاه   |   نسخه مرتبط   |   نشریه مرتبط   |   فهرست نشریات